The Fibers adopted by our company
are made by famous factaries from abroad. The relevant technical
specifications comply with or exceeds the ITU-T G.652B
recommendation.
|
|
|
|
1.Attenuation
Constant
|
|
|
|
|
|
2.Geometrical
Specifications
|
|
|
|
|
|
3.Chromatic
Dispersion
|
@1288-1339nm<=3.5ps/(nm.km)
|
@1271-1360nm<=5.3ps/(nm.km)
|
|
|
Zero Disp.WL. 1300-1324nm
|
Max.Zero Disp. 0.093ps/(nm.km)
|
|
|
|
4.Cutoff
Wavelength
|
λc =1150-1330nm(measured
in a 2m
fiber)
|
λcc<=1270nm(measured
in a 20m
fiber + 2m
cable )
|
|
5.bending
loss(dB)
|
radius 37.5mm,100
loose turns,at 1550nm<=0.05dB.
|
|
|
|
|
|
6.Fiber
mechanical strength test:
|
The fibers should
be proof tested over the whole length to an equivalent level og
stress of
|
more than 0.69Gpa(the strain
is about 1%)for 1 second.
|
|
|
|
7.Attenuation
lrregularity:
|
At the curve of
fiber's backward scatter,the attenuation value measured on any 500m fiber
|
subtract
the mean attenuation value measure every 500m over the whole length of
the fiber,and
|
the
worst value should not be more than 0.05dB.
|
|
|
|
8.Wavelength
induced attenuation
|
|
9.Polarization
mode dispersion coefficient(PMD)
|
|
|
|
<=0.2PS/√km
|
|
|
|
|
|
|
Note:
|
|
|
|
WL. : wavelength
|
M.F. : mode field
|
C.C. :core concentricity
|
|
Dia :diameter
|
Disp. :dispersion
|
Att. :attenuation
|
|
|
|
|
|
|
|
|
|
|
|